Originally Posted by hooverphonique View Post
so up to 73% is tin, indium and lead - where's the rest? :-)

They use cadmium, indium, bismuth tin and lead in their own recipe. I also bought a block of alloy that will melt in hot water... 46 deg Celcius... (also works out cheaper than buying chipquik... One third of the price

for info, Chipquik melts at 136 deg F ((58 deg C)

http://www.ebay.ca/itm/280998411099?...#ht_1793wt_898